Стандарты Британии (BS)
Стандарт
  • формат pdf
  • размер 304.5 КБ
  • добавлен 03 декабря 2011 г.
BS EN 288-4: 1992+A1: 1997 Specification and approval of welding procedures for metallic materials - Part 4 - Welding procedure tests for the arc welding of aluminium and its alloys
This European Standard was approved by CEN on 5 August 1992. Amendment A1 was approved on 1996-12-11. 30 р.

This standard specifies how a welding procedure specification is approved by welding procedure tests.
Похожие разделы
Смотрите также

AWS B5.17: 2004 Specification for the Qualification of Welding Fabricators (Eng)

Стандарт
  • формат pdf
  • размер 236.15 КБ
  • добавлен 12 января 2012 г.
This standard American Welding Society (AWS). 2004. 18p. This specification establishes the minimum requirements for the Welding Quality Program for Welding Fabricators (WF). This specification is intended to be used by companies regardless of the welding processes or materials used.

BS EN 1011-4: 2000+A1: 2003 Welding - Recommendations for welding of metallic materials - Part 4: Arc welding of aluminium and aluminium alloys (Eng)

Стандарт
  • формат pdf
  • размер 389.43 КБ
  • добавлен 18 декабря 2011 г.
This European Standard was approved by CEN on 14 August 2000, and amendment A1 was approved by CEN on 20 November 2003. 26p. This European Standard gives general recommendations for the manual, mechanized and automatic fusion welding of wrought and cast aluminium alloys and combinations thereof.

BS EN 14532-3: 2004 Welding consumables - Test methods and quality requirements - Part 3: Conformity assessment of wire electrodes, wires and rods for welding of aluminium alloys (Eng)

Стандарт
  • формат pdf
  • размер 431.74 КБ
  • добавлен 25 января 2012 г.
This European Standard was approved by CEN on 14 October 2004. 32p. This document describes the basic verification tests, the testing methods, the amount of testing and the requirements for the qualification of wire electrodes, wires and rods for welding of aluminium.

BS EN 288-1-1992+A1: 1997 Specification and approval of welding procedures for metallic materials - Part 1 - General rules for fusion welding

Стандарт
  • формат pdf
  • размер 107.57 КБ
  • добавлен 03 декабря 2011 г.
This European Standard was approved by CEN on 1992-02-21. Amendment A1 was approved on 1996-12-11. 14 р. This standard defines general rules for the specification and approval of welding procedures for metallic materials. This standard also refers to several other standards as regards detailed rules for specific applications.

BS EN 288-5: 1995 Specification and approval of welding procedures for metallic materials - Part 5 - Approval by using approved welding consumables for arc welding

Стандарт
  • формат pdf
  • размер 279.97 КБ
  • добавлен 03 декабря 2011 г.
This European Standard was approved by CEN on 1994-08-17. 12 р. This standard simplifies the approval of welding procedures especially for repetitive operations.

BS EN 288-7: 1995 Specification and approval of welding procedures for metallic materials - Part 7 - Approval by a standard welding procedure for arc welding

Стандарт
  • формат pdf
  • размер 223.98 КБ
  • добавлен 03 декабря 2011 г.
This European Standard was approved by CEN on 1995-04-07. 10 р. This standard defines the conditions for the approval of a standard welding procedure and establishes the conditions, limits and ranges of approval necessary for the use of standard welding procedures.

Grong O. Metallurgical Modelling of Welding

  • формат pdf, gif
  • размер 23.53 МБ
  • добавлен 15 января 2012 г.
The Institute of Materials, 1997, ISBN-10: 1861250363, 593 pages Welding metallurgy is concerned with the application of well-known metallurgical principles for assessment of chemical and physical reactions occurring during welding. On purely practical grounds it is nevertheless convenient to consider welding metallurgy as a profession of its own because of the characteristic non-isothermal nature of the process. In welding the reactions are fo...

Mathers G. The welding of aluminium and its alloys(Сварка Алюминия и его сплавов)

  • формат pdf
  • размер 3.66 МБ
  • добавлен 16 января 2011 г.
2002, - 236 p. The book provides a basic understanding of the metallurgical principles involved in how alloys achieve their strength and how welding can affect these properties. I have included sections on parent metal storage and preparation prior to welding and have also described the more frequently encountered processes. There are recommendations on welding parameters that may be used as a starting point for the development of a viable weldin...