BS EN 288-1-1992+A1: 1997 Specification and approval of welding procedures for metallic materials - Part 1 - General rules for fusion welding
This European Standard was approved by CEN on 1992-02-21.
Amendment A1 was approved on 1996-12-11. 14 р.

This standard defines general rules for the specification and approval of welding procedures for metallic materials. This standard also refers to several other standards as regards detailed rules for specific applications.
Похожие разделы
Смотрите также

AWS B5.17: 2004 Specification for the Qualification of Welding Fabricators (Eng)

Стандарт
  • формат pdf
  • размер 236.15 КБ
  • добавлен 12 января 2012 г.
This standard American Welding Society (AWS). 2004. 18p. This specification establishes the minimum requirements for the Welding Quality Program for Welding Fabricators (WF). This specification is intended to be used by companies regardless of the welding processes or materials used.

BS EN 1011-1: 1998+A1: 2002+A2: 2003 Welding - Recommendations for welding of metallic materials - Part 1: General guidance for arc welding (Eng)

Стандарт
  • формат pdf
  • размер 388.56 КБ
  • добавлен 18 декабря 2011 г.
This European Standard was approved by CEN on 26 January 1998 and amendment A1 was approved by CEN on 1 April 2002; amendment A2 was approved by CEN on 30 November 2003. 16p. This European Standard gives general guidance for fusion welding of metallic materials in all forms of product (e.g. cast, wrought, extruded, forged). The processes and techniques referred to in this part of EN 1011 may not all be applicable to all materials. Additional info...

BS EN 1011-4: 2000+A1: 2003 Welding - Recommendations for welding of metallic materials - Part 4: Arc welding of aluminium and aluminium alloys (Eng)

Стандарт
  • формат pdf
  • размер 389.43 КБ
  • добавлен 18 декабря 2011 г.
This European Standard was approved by CEN on 14 August 2000, and amendment A1 was approved by CEN on 20 November 2003. 26p. This European Standard gives general recommendations for the manual, mechanized and automatic fusion welding of wrought and cast aluminium alloys and combinations thereof.

BS EN 1011-5: 2003 Welding - Recommendations for welding of metallic materials - Part 5: Welding of clad steel (Eng)

Стандарт
  • формат pdf
  • размер 163.22 КБ
  • добавлен 18 декабря 2011 г.
This European Standard was approved by CEN on 28 February 2003. 14p. This European Standard gives general recommendations for welding of clad steels by means of appropriate arc welding processes and electroslag strip cladding. It is generally applicable to all clad steels and is appropriate regardless of the type of fabrication involved, although the application standard may have additional requirements. Non-ferrous claddings, such as titanium, t...

BS EN 1011-6: 2005 Welding - Recommendations for welding of metallic materials - Part 6: Laser beam welding (Eng)

Стандарт
  • формат pdf
  • размер 623.63 КБ
  • добавлен 18 декабря 2011 г.
This European Standard was approved by CEN on 28 November 2005. 44p. This European Standard gives general quidance fir laser beam welding and associated processes of metallic materials inallforms of product (e.g. cast, wrought, extruded, forged).

BS EN 288-4: 1992+A1: 1997 Specification and approval of welding procedures for metallic materials - Part 4 - Welding procedure tests for the arc welding of aluminium and its alloys

Стандарт
  • формат pdf
  • размер 304.5 КБ
  • добавлен 03 декабря 2011 г.
This European Standard was approved by CEN on 5 August 1992. Amendment A1 was approved on 1996-12-11. 30 р. This standard specifies how a welding procedure specification is approved by welding procedure tests.

BS EN 288-5: 1995 Specification and approval of welding procedures for metallic materials - Part 5 - Approval by using approved welding consumables for arc welding

Стандарт
  • формат pdf
  • размер 279.97 КБ
  • добавлен 03 декабря 2011 г.
This European Standard was approved by CEN on 1994-08-17. 12 р. This standard simplifies the approval of welding procedures especially for repetitive operations.

BS EN 288-7: 1995 Specification and approval of welding procedures for metallic materials - Part 7 - Approval by a standard welding procedure for arc welding

Стандарт
  • формат pdf
  • размер 223.98 КБ
  • добавлен 03 декабря 2011 г.
This European Standard was approved by CEN on 1995-04-07. 10 р. This standard defines the conditions for the approval of a standard welding procedure and establishes the conditions, limits and ranges of approval necessary for the use of standard welding procedures.

Deyev G.F., Deyev D.G. Surface Phenomena in Fusion Welding Processes

  • формат pdf
  • размер 14.67 МБ
  • добавлен 05 января 2012 г.
CRC Press, Taylor & Francis Group, 2006, Pages: 407 The manufacturing industry currently employs a wide variety of welding processes. The main technological process applied in the production of weldments is fusion welding. Presenting the latest research on the topic, Surface Phenomena in Fusion Welding Processes is a cutting-edge and comprehensive book that details the various courses of action that occur during welding procedures. It expl...