Reed R.C. The Superalloys: Fundamentals and Applications
Cambridge University Press, 2006, ISBN: 0521859042, 372 pages

Superalloys are unique high-temperature materials used in gas turbine engines, which display excellent resistance to mechanical and chemical degradation. This book presents the underlying metallurgical principles which have guided their development and practical aspects of component design and fabrication from an engineering standpoint. The topics of alloy design, process development, component engineering, lifetime estimation and materials behaviour are described, with emphasis on critical components such as turbine blading and discs. The first introductory text on this class of materials, it will provide a strong grounding for those studying physical metallurgy at the advanced level, as well as practising engineers. Included at the end of each chapter are exercises designed to test the reader's understanding of the underlying principles presented.

Introduction
The physical metallurgy of nickel and its alloys
Single-crystal superalloys for blade applications
Superalloys for turbine disc applications
Environmental degradation: the role of coatings
Summary and future trends
Смотрите также

Appel F., Paul J.D.H., Oehring M. Gamma Titanium Aluminide Alloys: Science and Technology

  • формат pdf
  • размер 14.67 МБ
  • добавлен 02 октября 2011 г.
Wiley-V.C.H, 2011. 745 p. This first book entirely dedicated to titanium aluminide alloys emphasizes the relation between basic research topics and processing technologies for real applications. As such, it covers complex microstructures down to the nanometer scale, titanium aluminide structure/property relationships and the potential in such key industries as aerospace, automotive and power conversion. The result is more detailed coverage of t...

ASM Metals HandBook Vol. 13 - Corrosion: Fundamentals, Testing, and Protection

  • формат pdf
  • размер 79.01 МБ
  • добавлен 17 февраля 2011 г.
ASM International, 2002, 2597 p. ASM Handbook, Volume 13A, Corrosion: Fundamentals, Testing, and Protection, is the first volume in a two-volume update, revision, and expansion of Corrosion, Volume 13 of the ninth edition Metals Handbook, published in 1987. The second volume—ASM Handbook, Volume 13B, Corrosion: Materials, Environments, and Industries—is to be published in 2005. The purpose of these two volumes is to represent the current state o...

ASM Metals HandBook Vol. 15 - Casting

  • формат pdf
  • размер 48.79 МБ
  • добавлен 17 февраля 2011 г.
ASM International, 2002, 2002 p. The Handbook is structured in ten Sections, along with a Glossary of Terms. The reader is first introduced to the historical development of metal casting, as well as to the advantages of castings over parts produced by other manufacturing processes, their applications, and the current market size of the industry. Then, the thermodynamic relationships and properties of liquid metals and the physical chemistry of g...

ASM Metals HandBook Vol. 2 - Properties and Selection: Nonferrous Alloys and Special - Purpose Materials

  • формат pdf
  • размер 63.08 МБ
  • добавлен 16 февраля 2011 г.
ASM International, 2002, 3470 p. This is the second of two volumes in the ASM Handbook that present information on compositions, properties, selection, and applications of metals and alloys. In the first volume, irons, steels, and superalloys were described. In the present volume, nonferrous alloys, superconducting materials, pure metals, and materials developed for use in special applications are reviewed. In addition to being vastly expanded...

Davis J.R. (Ed.) Heat Resistant Materials

  • формат pdf
  • размер 131.16 МБ
  • добавлен 15 января 2012 г.
ASM International, 1997, ISBN: 0871705966, Pages: 591 ASM Speciality Handbook This latest handbook brings together in one volume a comprehensive reference source of information on engineering metallic and nonmetallic heat-resistant materials from carbon and alloy steels to refractory metals, and ceramics to carbon-carbon composites. The volume covers the complete spectrum of technology dealing with heat-resistant materials including high-tempe...

Groover M.P. Fundamentals of Modern Manufacturing, Vol. 1 and 2

  • формат pdf, jpeg
  • размер 69.01 МБ
  • добавлен 05 января 2012 г.
3 Edition, John Wiley, 2007, 1040 pages, ISBN: 0471744856 A modern, all-inclusive look at manufacturing In this modern, quantitative approach to manufacturing, Mikell Groover offers balanced coverage of the three basic engineering materials––metals, ceramics, polymers, as well as composites––along with recently developed manufacturing processes and electronics manufacturing technologies. Throughout Fundamentals of Modern Manufacturing, the...

Moiseyev V.N. Titanium Alloys- Russian Aircraft and Aerospace Applications

  • формат pdf
  • размер 21.09 МБ
  • добавлен 03 октября 2010 г.
2006. Taylor and Francis, LLC. p. 196. The publication of Titanium Alloys in Russia: Aircraft and Aerospace Applications offers previously elusive information on state-of-the-art Russian metallurgic technology of titanium alloys. It details their physical, mechanical and technological properties, as well as treatments and applications in various branches of modern industry, particularly aircraft and aerospace construction. This inaugural book a...

Ohring M. Engineering Materials Science

  • формат pdf
  • размер 76.11 МБ
  • добавлен 31 января 2012 г.
Academic Press, 1995, 827 pages, ISBN: 0125249950 Milton Ohring's Engineering Materials Science integrates the scientific nature and modern applications of all classes of engineering materials. This comprehensive, introductory textbook will provide undergraduate engineering students with the fundamental background needed to understand the science of structure-property relationships, as well as address the engineering concerns of materials sele...

Polmear I. Light Alloys: From Traditional Alloys to Nanocrystals

  • формат pdf
  • размер 9.23 МБ
  • добавлен 18 января 2012 г.
4th Edition,Butterworth-Heinemann, Elsevier, 2006, ISBN: 0750663715, Pages: 421 The definitive overview of the science and metallurgy of aluminum, magnesium, titanium and beryllium alloys, this is the only book available covering the background materials science, properties, manufacturing processes and applications of these key engineering metals in a single accessible volume. Use of these metals is now more widespread than ever, and they are r...

Smallman R.E., Bishop R.J. Modern Physical Metallurgy and Materials Engineering: Science, process, applications

  • формат pdf
  • размер 8.6 МБ
  • добавлен 20 января 2012 г.
6 edition, Butterworth - Heinemann, 1999, 438 pages, ISBN: 0750645644 For many years, various editions of Smallman's Modern Physical Metallurgy have served throughout the world as a standard undergraduate textbook on metals and alloys. In 1995, it was rewritten and enlarged to encompass the related subject of materials science and engineering and appeared under the title Metals & Materials: Science, Processes, Applications offering a compre...